- All
- Favorite
- Popular
- Most rated
- Expired
Divided into processed tin bronze and cast tin bronze. The tin content of tin bronze used for pressure processing is less than 6% to 7%, and the tin content of cast tin bronze is 10% to 14%. Commonly used grades are QSn4-3, QSn4.4-2.5, QSn7-O.2, ZQSn10, ZQSn5-2-5, ZQSN6-6-3, etc.
Continuous casting tin bronze rod CC480K as per EN Standard CuSn10-C
- 1:In Chemical Composition, Single values represent maximums.
- 2:Mechanical performance of hardness value is only for reference.